Evident LogoOlympus Logo
Zdroje informací
Application Notes
Back to Resources

Step measurement of transparent film applied to a glass surface


Microscopic shape measurement using a laser microscope

1. Application

Transparent materials are used in various manufacturing processes for electronic equipment, semiconductors and electronic components, and basic research. One common application is to measure the height (step) of a film from the glass substrate to which the transparent film has been applied. Because the thickness of a coated film greatly affects the performance and functionality of the resulting product, it is important to measure the thickness of the film after it has been applied to make sure it is the correct height.

Measuring the height of a transparent film has long been a challenge. Using an optical microscope to evaluate the surface profile of a film is difficult because the film’s transparency makes it very difficult to focus. In addition, since the materials are non-conductive, it is also difficult to observe the film using an electron microscope, which requires a metal film to be deposited on the surface. Contact-type step testers are also problematic because the stylus can damage the surface of the film.

2. The Olympus solution

With the LEXT 3D laser scanning microscope, the reflected light focused by the confocal optical system can be extracted so that even the reflection from a transparent film surface with low reflectivity can be captured by the high-sensitivity detector. Most importantly, the microscope uses laser light to enable reliable non-contact surface profile measurements without damaging the sample.

Images

(1) Step of one transparent film layer : 7.095 μm

Step of transparent film 1×coating ob20X

(2) Step of one + two transparent film layer : 28.819 μm

Step of transparent film 2×coating ob20X

(3) Step of one + two + three transparent film layer  36.739 μm

Step of transparent film 3×coating ob20X
 

Olympus IMS

Produkty použité pro tuto aplikaci

The LEXT™ OLS5100 laser scanning microscope combines exceptional accuracy and optical performance with smart tools that make the system easy to use. The tasks of precisely measuring shape and surface roughness at the submicron level are fast and efficient, simplifying your workflow and delivering high-quality data you can trust.

Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.
Sorry, this page is not available in your country