Phased array testing helps make corrosion inspection fast and efficient. Our solutions enable inspectors to be more productive and collect higher resolution data with fully encoded C-scan imaging.
The HydroFORM® scanner, FlexoFORM™ scanner, RexoFORM wedge, and Dual Linear Array™ probe offer efficient inspection options for detecting loss of wall thickness due to corrosion, abrasion, and erosion. Our solutions can also detect mid-wall damage, such as hydrogen-induced blistering or manufacturing-induced laminations, and easily differentiate these anomalies from loss of wall thickness.
|
| ||
|
|
| ||
|
|
|
DLA corrosion | FlexoFORM | HydroFORM | RexoFORM | RollerFORM | |
Phased array probe | REX1 | FA1 | 7.5L64-I8 | A12, A14 | WP1 |
Maximum one-line scan coverage (width) | 32 mm | 64 mm | 60 mm | 38 mm (A12), 60 mm (A14) | 51.2 mm |
Delay line medium | Rexolite | Water | Water | Rexolite | Water/acoustic polymer |
Delay line height | 7.7 mm | 9 mm | 14 mm or 38 mm | 20 mm | 25 mm |
Position of 2nd interface echo (in steel) | N/A | 34 mm |
Short plate: 54 mm
Tall plate: 114 mm | 50 mm | 28 mm |
Max. recommended thickness (in steel) | 80 mm | 30 mm |
50 mm (14 mm delay line)
150 mm (38 mm delay line) | 46 mm | 25 mm |
Typical near-surface resolution (1/8 in. FBH) | 1 mm | 2 mm | 1.5 mm | 2 mm | 3 mm |
OD inspection range | 4 in. and greater | 4.5 in. and greater | 4 in. and greater | 4 in. and greater | 4 in. and greater |
ID inspection range | N/A | N/A | 10 in. and greater (16 in. with index encoder) | N/A | 20 in. and greater |
Contact device with surface | Carbides | Wheels | Wheels | Carbides | Wheels |
Footprint | 40 mm × 65 mm | 92 mm × 230 mm | 110 mm x 130 mm | 40 mm x 95 mm | 144 mm × 144 mm |
Scan direction | Circumferential | Longitudinal | Circumferential | Circumferential | Longitudinal and Circumferential |
Scan speed at 1 mm x 1 mm resolution | 300 mm/s | 123 mm/s | 123 mm/s | 123 mm/s | 123 mm/s |
![]() | OmniScan MXU software displaying A-scan, S-scan, and C-scan views of corrosion. The OmniScan software has a full range of tools and displays for corrosion mapping applications:
|
![]() | TomoView software displaying A-scan, S-scan, and C-scan views of corrosion. Computer-based data analysis software with a full range of corrosion evaluation features:
|
You are being redirected to our local site.