Tired of Removing Paint to Inspect Welds?

By  -

Removing Paint is Time Consuming and Expensive

For decades, legacy NDT methods, such as penetrant and magnetic particle inspection, required that paint be removed from parts before they could be inspected. The paint was often removed using harsh chemicals. Over time, increasingly strict government regulations about chemical safety and waste treatment have caused the cost of paint removal to rise dramatically. As the cost of paint removal increases so does the overall cost of inspection.

Inspect Through Paint with Dynamic Lift-Off Compensation Technology

The use of a flexible PCB probe with cross-wound coil technology combined with dynamic lift-off compensation makes it possible to detect surface-breaking cracks through paint, resulting in significant time and cost savings.

The principle of dynamic lift-off compensation
The principle of dynamic lift-off compensation.
 

Our MagnaFORM™ probe features dynamic lift-off compensation and helps make weld inspection fast and efficient. The dynamic lift-off compensation helps the probe maintain sensitivity to surface-breaking cracks. All of the channels perform lift-off compensation in real time. Now, we can inspect through paint up to 3 mm thick.

The MagnaFORM probe
The MagnaFORM probe.
 

The MagnaFORM probe enables you to inspect through painted surfaces
The MagnaFORM probe enables you to inspect through painted surfaces.
 

The MagnaFORM Probe Delivers Results

The example below demonstrates that the MagnaFORM probe provides you with clear images through paint for indications with the same lengths and same depths located on different areas of welded parts. The amplitude of the signals is the same for each location, demonstrating consistent defect detection in all locations.

A C-scan image using a MagnaFORM probe of EDM notch indications at different locations
A C-scan image using a MagnaFORM probe of EDM notch indications at different locations.
 

Don't spend valuable resources on stripping and repainting surfaces as part of your inspection process. With eddy current array technology and the advanced features of the MagnaFORM probe, you can inspect welds and surfaces through paint, helping you save time and reduce cost. To learn more, check out this video about the MagnaFORM solution.


Get In Touch
Product Leader, Eddy Current Product Line

Since 2012, Ghislain Morais has been an eddy current and bond testing product leader for Evident. He is responsible for the global support of conventional eddy current, eddy current array, conventional bond testing, and bond testing C-scan technology. Prior to joining us, he spent 18 years working in the aircraft maintenance business as a metallurgist and in NDT inspections. He has experience and certifications in several of the NDT methods that are used in the aerospace industry.

březen 14, 2017
Sorry, this page is not available in your country
InSight Blog Sign-up
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.
Sorry, this page is not available in your country