Evaluating the Coating on a Smartphone Housing / Film thickness measurement and 3D surface profile measurement using a laser microscope


Application

To sell successfully, the latest electronic equipment, such as smartphones, must be both functional and attractive. Customers want products that look good and have a pleasant feel and surface texture. Manufacturers apply a clear coating to improve the durability of smartphone’s painted surfaces. This means that the surface of a smartphone housing has a two-layer coating: a color coating and a clear coat. Manufacturers must inspect the thickness and surface profile of both the color and clear coats to ensure a high-quality product.

The Olympus solution

Olympus' LEXT 3D scanning laser microscope is used to measure the thickness of films including color and clear coats. The microscope enables users to identify the peak amount of reflected light for multiple layers and detect the position of each layer. With these features, users can accurately measure the film thickness of a transparent layer. With the microscope’s multi-layer function, users can also obtain surface profile data for the top transparent layer as well as the material beneath to measure each layer’s roughness.

Surface of a transparent coating film

transparent_coating_film_surface_objective20X_zoom1X

3d_transparent_coating_film_surface_objective20X_zoom1X

Objective lens 20X, Zoom 1X

Surface of a color coating layer

surface_of_a_lower_color_coating_layer_objective20X_zoom1X

Objective lens 20X, Zoom 1X

3d_surface_of_a_lower_color_coating_layer_objective20X_zoom1X

Film thickness measurement

Film thickness measurement

Olympus IMS

Verwendete Produkte

The LEXT™ OLS5100 laser scanning microscope combines exceptional accuracy and optical performance with smart tools that make the system easy to use. The tasks of precisely measuring shape and surface roughness at the submicron level are fast and efficient, simplifying your workflow and delivering high-quality data you can trust.

Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.
Sorry, this page is not available in your country