Application

Fabrics used for clothing are broadly categorized into natural fibers (cotton, linen, wool, cashmere) and chemical fibers (acrylic, polyester). The fiber’s surface condition affect its absorbability, hygroscopicity, heat retention, dye-affinity, and texture. Managing the surface profile of these fibers down to the micron level becomes significant when it comes to enhancing the performance and quality of the fibers.
The surface profile of a fiber is so minute that it is usually observed using an electron microscope. However, electron microscopes require time-consuming sample preparation steps, and they are not very good for quantitative evaluations, such as surface roughness. Because the fibers are very delicate, manufacturers require a method for evaluating the fiber’s quality with minimal sample preparation so that the fibers are not damaged.

The Olympus solution

Olympus' LEXT 3D scanning laser microscope enables users to make three-dimensional observations and roughness measurements of the surface of a fiber. The LEXT features dedicated objective lenses with high numerical apertures and an optical system that obtains maximum performance from the 405 nm laser so it can clearly capture the profile of a curved fiber surface without causing damage.

Human hair

human_hair_50X

Objective lens 50X  

Wool

wool_50X

Objective lens 50X

Cashmere

cashmere_50X

Objective lens 50X

Polyester

polyester_50X

Objective lens 50X  

Acrylic

acrylic_50X

Objective lens 50X

Olympus IMS

Productos para la aplicación
NEW

El microscopio de escaneo láser LEXT™ OLS5100 combina precisión y rendimiento óptico a un nivel excepcional junto con herramientas inteligentes que facilitan su uso. Las tareas de medición precisa y submicrométrica con respecto a la forma y la rugosidad superficial son rápidas y eficientes, lo que simplificará su flujo de trabajo y proporcionará datos de alta calidad en los que puede confiar.

Lo sentimos, la página solicitada no se encuentra disponible en su país.
Let us know what you're looking for by filling out the form below.
Lo sentimos, la página solicitada no se encuentra disponible en su país.