Application: Measurement of individual layers and total thickness in coextruded plastic, both raw sheet stock and molded products.

Background: Sheet stock of engineering thermoplastics such as acrylonitrile butadiene styrene (ABS) and acrylic, used to form a wide variety of molded consumer products such as automotive interior parts, refrigerator shelves, and plastic window frames, is sometimes produced as two coextruded layers, an outer cap layer that provides cosmetic properties such as a glossy surface, and a base layer that optimizes structural properties. Manufacturers and fabricators need to measure the thickness of the cap layer as well as total product thickness to insure compliance with specifications.
Equipment: It is often possible to measure cap layer, base layer, and total thickness both in the sheet stock and in the final molded product using a Model 38DL PLUS thickness gage with the optional Multi-Measurement software and a common delay line transducer such as an M208-RM (20 MHz) or an M202-RM (10 MHz). Cap layers may often be measured down to a minimum thickness of 0.008 in. (0.20 mm) or less. The primary limitation on ultrasonic testing of this class of products is that occasionally the cap layer and base layer are both made materials with very similar acoustic properties, in which case there can be insufficient reflection from the boundary between them to measure the layers separately. For this reason, performance should be evaluated on samples of the actual product to be measured. Total product thickness can be measured in all cases.

Typical Procedure: The waveforms below show simultaneous measurement of cap layer and base layer in a typical coextruded ABS plastic part, using an M208 transducer. The echoes seen on the screen represent the outer surface of the part, the boundary between the cap layer and the base layer, and the inner surface of the part.

cap layer measurement
cap layer measurement


base layer measurement
base layer measurement

As with any ultrasonic thickness measurement, accuracy is dependent on proper sound velocity calibration. Velocity calibration must be performed for each material being measured, on samples of known thickness.

Olympus IMS

Productos para la aplicación

El 45MG es un avanzado medidor de espesores ultrasónico que cuenta con funciones de medición de serie y opciones de software. Está exclusiva herramienta de medición de espesores es compatible con nuestro rango completo de sondas duales y monoelementos dedicadas a medir espesores.

El versátil medidor de espesores 38DL PLUS™ puede ser usado con sondas duales para medir el espesor de tuberías corroídas, como también para ejecutar mediciones de espesor muy precisas de materiales delgados o multicapa mediante el uso de una sonda monoelemento. 
Lo sentimos, la página solicitada no se encuentra disponible en su país.
Let us know what you're looking for by filling out the form below.
Lo sentimos, la página solicitada no se encuentra disponible en su país.