Handheld XRF for FAC Corrosion Prediction by Cr in Carbon Steel


The DELTA Takes Detection Limits of Chromium (Cr) in Carbon Steel to an All Time Low!

It has been shown that small amounts of Cr in carbon steel pipes significantly reduce the rate of flow accelerated corrosion. Consequently, highly accurate measurements of low levels of Cr in carbon steel are critical for predicting the end of life in these pipes. In general, Cr is present in carbon steels as a residual tramp element ranging from 0 to 0.25%. The critical level of Cr monitored for FAC prediction is at about 0.04% (400ppm). The DELTA Premium, the latest development in HHXRF, goes to an all time high in accuracy and an all time low in detection limits for Cr and other metals. It detects trace levels of Cr as low as 0.004% (40ppm) in alloys; and 0.01% (100ppm) in carbon steel for FAC inspections. Although HHXRF is a non-destructive technique, accurate low Cr analysis of in-service and oxidized pipes can require some sample preparation to remove surface material before measurements. Portable angle grinders with alumina grinder disks are recommended.

power plant smoke stack

Comparison of DELTA Premium Handheld XRF with Certified Assays of Trace Cr in Carbon Steel

Standard Certified %Cr HHXRF Measured %Cr HHXRF %Cr +/-
IARM 229A 0.015 0.015 0.002
IARM 28E 0.079 0.080 0.005
IARM 33D 0.139 0.139 0.006
IARM 35F 1.160 1.210 0.006

DELTA Premium Analysis Time: 120sec Beam 1; 30 sec Beam 2

corrosion car steel DELTA accuracy chart

Delta Handheld XRF Analyzer in hip holster

Excellent Accuracy and Low Levels of Detection are Critical for Predicting Accelerated Corrosion

In addition to testing for flow accelerated corrosion, the power supply industry depends on HHXRF analyzers for startups, shutdowns, general maintenance, and trouble shooting. Managers cannot afford to depend on out-of-date and unreliable equipment, or untimely support of equipment. They also cannot afford to fall behind the technology curve. The analytical capabilities of HHXRF continue expanding, and new features continually enable operators to be more effective and efficient. Upgrade your HHXRF to the DELTA - the latest HHXRF loaded with innovative features and backed by the industry's best service and support.

Handheld XRF for Metals & Alloys Industries

Iron & Steel Non-ferrous Scrap & Secondary

Iron and steel are the most widely used of metals and alloys. Lighter metals, non-ferrous, newly developed and exotic alloys are also utilized extensively, but iron and steel are considered the basic raw materials for the majority of industrial goods and construction. Although produced from ores mined around the globe, steel is one of the most recycled materials in the world. From base form to recycled materials to finished products, metals and alloys are integral to the fabric of society, the consumption of which is often considered a primary indicator of development and economic progress.

Metals Alloys is a serious, dynamic business.

The DELTA XRF analyzer is an essential tool for all businesses involved in the trade or use of metals alloys. In seconds, you can nondestructively measure 25+ elements. Turnings, shavings, rods, wires, small parts, components, sizeable materials and large structures can all be analyzed directly, non-destructively. How you get them, how you make them, how you use them, how you sell them is how you measure them. Whether you check purity, chemistry, or grade ID for highest value, maximum recovery, quality, conformance, or maintenance and safety, our DELTA XRF analyzer will give you immediate answers to take action on now.

Delta Handheld XRF testing for alloys
Olympus IMS

Productos para la aplicación
Los analizadores XRF portátiles DELTA, dedicados a la identificación positiva del material (PMI), permiten analizar aleaciones de forma no destructiva para identificar con rapidez y precisión los grados de las aleaciones y medir la composición de los metales. Efectúe inspecciones PMI y ensayos de control/aseguramiento de calidad, que cubren desde una identificación simple de grados, en conformidad con las especificaciones del control de calidad, hasta inspecciones de materiales entrantes y verificaciones de productos finales.
El DELTA Element es un analizador de fluorescencia de rayos X (XRF) económico y de alto rendimiento que ha sido optimizado para las aplicaciones de clasificación de chatarra, identificación positiva de los materiales (PMI), control y aseguramiento de calidad de aleaciones (QA/QC), y análisis de metales preciosos.
El DELTA Professional, dotado de un detector de deriva de silicio (SDD) de gran superficie y tubo de rayos X avanzado de 4W, proporciona un rendimiento superior en términos de velocidad, límites de detección y escala de elementos. Analiza elementos que van desde el magnesio (Mg) hasta elementos superiores en aleaciones y minerales. Este analizador representa la mejor solución de la serie de analizadores DELTA de Olympus.
Lo sentimos, la página solicitada no se encuentra disponible en su país.
Let us know what you're looking for by filling out the form below.
Lo sentimos, la página solicitada no se encuentra disponible en su país.