High-Speed Phased Array Ultrasound Inspection of Aerospace Composite Parts


Background

Over the past decade, the aviation market has experienced a sustained period of significant growth. Global air traffic has risen at a steady rate, and commercial and military airplane manufacturers have undertaken several major programs (including the A350, A380, B787, and B777). This development has been consistent despite ever-increasing fuel prices and growing environmental concerns over emissions.

Performance demands on aircraft manufacturers and their suppliers have intensified. High fuel prices and an increased focus on the environment have led manufacturers to develop lightweight materials in order to build more efficient aircraft. Increased air traffic and the introduction of new airplane models has put pressure on the suppliers to maximize productivity, which can be achieved, in part, through faster inspection speeds.

High-speed inspection of composite parts is particularly difficult because of the complex geometries that are involved.

Problem

In production environments, manufacturers of composite parts are facing the challenge of having to inspect complex-shaped parts at very fast inspection speeds.

Complex Geometry Inspection
Composite parts often feature complex geometries that require full volumetric coverage, therefore requiring more advanced inspection techniques to be used.

Fast Inspection Speed
The constant increase in the production rates of commercial and military aircraft puts more and more pressure on the quality control process to be performed at higher speeds.

Solution

To meet these challenges, Olympus offers an integrated, nondestructive inspection solution comprising hardware (acquisition unit), multiple phased array probes, and dedicated software, all designed for high-performance inspection.

Multiple-Probe Configurations
Multiple phased array probes are required to help ensure full volumetric coverage in a single inspection on complex-shaped composite parts. The FOCUS PX acquisition instrument has the capability to drive numerous probes and bring all the data together in FocusPC software, greatly simplifying the inspection process, reducing cycle time, and improving operator efficiency.

Multiple-Probe Configurations

High-Performance Acquisition Unit
The FOCUS PX acquisition instrument enables you to build significantly faster and more efficient inspection systems by taking advantage of its high-end specifications.

  • Scalability (use up to four FOCUS PX units in parallel)
  • High pulse repetition frequency (PRF)
  • High data throughput
  • 5 gates with advanced synchronization capabilities
FOCUS PX

Powerful and Flexible Software
The FocusPC software is designed with powerful inspection and analysis features to take full advantage of the FOCUS PX unit’s capabilities and help ensure optimal system performance. FocusPC software can be easily integrated into typical industry software environments and offers multiple advanced composite inspection features.

  • Signal-to-noise ratio (SNR) analysis
  • Easy and precise delamination sizing
  • Matrix filters
  • C-scan merge
High Performance Acquisition Unit

Scalability
The FocusPC software has the capability to drive up to four FOCUS PX acquisition units in parallel, enabling improved coverage and up to a threefold increase in inspection speed. Also, having all the inspection data from the multiple FOCUS PX units gathered in the customizable FocusPC software display helps to improve operator efficiency.

ScalabilityScalability

System Automation
The FOCUS PX software development kits (SDK) can also be used to automate the inspection process and build application-dedicated software, further improving cycle and operator efficiency.

System Automation

Conclusion

Olympus’ advanced inspection technologies enable the development of high-performance inspection solutions that can be used to achieve full volumetric coverage on complex-shaped parts while helping ensure optimal inspection speed.

Olympus IMS

Productos para la aplicación

La unidad de adquisición extensible FOCUS PX junto con el software FocusPC otorgan lo último en tecnología de ultrasonido multielemento (Phased Array) y ultrasonido convencional a fin de facilitar su integración en sistemas automatizados y semiautomatizados. Las capacidades de la unidad FOCUS PX y de su software para generar y guardar datos C-scan y A-scan sin tratar los vuelve la elección idónea para aplicaciones cuyo veredicto de inspección se emite por medio de análisis de datos posteriores a la inspección. Estas aplicaciones destacan en la industria aeroespacial (laminado de compuestos), de generación de energía (álabes eólicos), transporte (ruedas de trenes), metalúrgica (piezas forjadas) y más.

Los kits de desarrollo de software (SDK) opcionales FocusControl, FocusData y OpenView son compatibles con la unidad FOCUS PX para que los clientes puedan desarrollar su propio software de aplicación.

Lo sentimos, la página solicitada no se encuentra disponible en su país.
Let us know what you're looking for by filling out the form below.
Lo sentimos, la página solicitada no se encuentra disponible en su país.