Evident LogoOlympus Logo
Documentation
Notes d’application
Retour aux ressources

Cracking in Ceramic Diesel Particulate Filters


EPOCH XT testing ceramic

Application
Detection of internal cracking in ceramic diesel particulate filters.

Background
The use of ceramic particulate filters is well established as a method for removing environmentally dangerous soot and similar particulates from diesel engine exhaust, especially for diesel engines used in trucks and buses. These filters have the form of large cylinders, approximately 100 mm to 300 mm (4 in. to 12 in.) in diameter and 150 mm to 350 mm (6 in. to 14 in.) high. They are commonly made of cordierite, silicon carbide, or ceramic in a fine honeycomb pattern. As the hot exhaust is forced through the porous filter under pressure, soot particles collect on the surfaces of the honeycomb channels where they then break down or oxidize due to heat.

These complex ceramic structures can potentially crack during manufacturing, handling, or in service, causing reduced performance or failure that can cause both environmental and engine damage. Ultrasonic testing can quickly and nondestructively detect internal cracking in both new and used ceramic filter elements. The technique usually requires access to only one end of the cylinder.

Equipment
This test can be performed with both conventional flaw detectors and phased array instruments Any of the Epoch-series flaw detectors (EPOCH LTCEPOCH 600, EPOCH 650 or Epoch 1000) can be used with a low frequency contact transducer such as an A601S-RB or V601-RB (500 KHz). The OmniScan SX can also be used with the aforementioned transducers. A soft polymer membrane on the face of the transducer is used to couple sound energy into the filter without the need for liquid couplants that could be difficult to remove. The Advanced Filter option (standard on the Epoch 1000) can be helpful for improving signal-to-noise when testing larger filters by improving the instrument's low frequency response. Phased array testing can be performed with the OmniScan or Epoch 1000 and 1.5 MHz probes such as the 1.5L16-A4.

Procedure
Using firm hand pressure, the transducer is coupled to the end of the filter. High frequency sound energy propagating as plate waves travels through the ceramic honeycomb, reflecting off the far end if there are no discontinuities. If there is a crack parallel to the end surface, an echo will be received ahead of the point on the display representing the far end of the filter. If there is a crack that is tilted with respect to the ends, there may be no direct reflection but the echo from the far end will disappear.
 

In the example below representing a setup with a flaw detector and an A601S-SB transducer, the left screen image represents a typical echo pattern from an undamaged filter. The peaks at the left side of that waveform represent reverberations of the outgoing sound pulse, and the echo at the right side represents the reflection from the far end. There should be no significant echoes in the zone in the middle that is marked by the red gate. The right screen image represents an echo pattern from a filter that is cracked just past its midpoint. The backwall echo to the right of the gate has disappeared because sound energy is no longer reflecting from the far wall. The transducer can be moved to as many points as desired on the face of the filter to check for cracks at other locations.

Typical Backwall Echo from Good Filter

Typical Backwall Echo from Good Filter

Typical Midwall Echoes from Cracked Filter

Typical Midwall Echoes from Cracked Filter

The specific instrument setup for each type of filter should be established through the use of a known good setup standard that is used to optimize the echo from the far end. By identifying the echo pattern from a good filter and looking for changes, a trained operator can quickly and reliably identify echo variations that correspond to internal cracks.

Phased Array Testing

OmniScan Testing

Phased Array can offer cross-sectional imaging of filters from either sectorial or linear scans. This can aid operator visualization of flaws. Automated testing has also been implemented using larger array probes and specialized fixturing.

Olympus IMS

Produits utilisés pour cette application
L’OmniScan PA effectue des inspections multiéléments manuelles et automatisées. Il offre toutes les fonctionnalités d’affichage du A-scan, du B-scan, du S-scan et du C-scan, ainsi que le traitement de données de pointe et en temps réel. Configuration de base des éléments 16:128, configurations possibilités de 16:16M, 16:64M, 32:32 et 32:128
De conception compacte et légère, l’OmniScan SX effectue des inspections économiques à un seul groupe en plus d’offrir une nouvelle interface utilisateur simplifiée sur écran de 8,4 po. L’appareil est offert en deux modèles distincts : SX PA et SX UT. Le modèle SX PA est une unité multiélément 16:64PR et, tout comme le modèle SX UT, il est équipé d’un canal UT conventionnel pour les inspections TOFD, par réflexion ou par émission-réception séparées.
Chaque appareil de la série OmniScan™ X3 constitue en lui-même un coffre à outils complet pour l’inspection multiélément. Des capacités TFM innovantes et PA avancées vous aident à identifier les défauts en toute confiance, tandis que des outils logiciels puissants et des flux de travaux simples améliorent votre productivité.
L’EPOCH 650 est un appareil de recherche de défauts par ultrasons conventionnels très performant adapté à un grand nombre d’applications. Cet appareil intuitif et robuste remplace le populaire appareil de recherche de défauts EPOCH 600. Il est aussi doté de fonctionnalités supplémentaires.
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.
Sorry, this page is not available in your country