Detection of Accelerated Corrosion with Handheld X-ray Fluorescence


Introduction

Crude oil generally contains only 10-40% the hydrocarbon constituents in gasoline. Refineries process crude oil using fluid catalytic cracking unit (FCCU) processes to convert high molecular weight hydrocarbons into smaller, more volatile compounds such as propene and butene. The latter, are converted using hydrofluoric acid (HF) as a catalyst to obtain liquid gasoline-sized hydrocarbons (alkylates). Alkylate is composed of a mixture of high octane branched chain paraffinic hydrocarbons (isoheptane and isooctane). Alkylate is a premium gasoline blending stock which provides antiknock properties and clean burning. These processes need to stay contained within carbon steel pipes that run throughout the refinery.

hf steel industrial clouds

X-Ray Fluorescence (XRF) accurately detects low levels of corrosion indicative elements such as Cr, Ni, and Cu in these aforementioned carbon steel pipes. Detection of these indicative residuals is critical for predicting accelerated corrosion within a petrochemical plant. In addition to testing for trace levels of corrosion indicative residuals, the petrochemical industry depends on handheld XRF analyzers for material inspection startups, shutdowns, general maintenance and trouble shooting. Managers cannot afford to depend on out-of-date and unreliable equipment, or fall behind the technology curve. The analytical capabilities of XRF continue to expand, while new features enable operators to be more effective and efficient.

Delta Handheld XRF in docking station

Application detail

DELTA handheld XRF analyzers provide highly accurate measurements of low levels of Cr, Ni and Cu in carbon steel are critical for predicting accelerated corrosion of components in HF Alkylation process units. It has been shown that if the sum of the residuals, Cr, Ni and Cu, exceeds 0.20%, the carbon steel components used in HF Alkylation processes will likely experience a preferentially accelerated corrosion rate. In general, a level between 0.15% and 0.20% of the sum of the three key residuals is deemed optimal, depending on the component, its use and location in the unit. As this is a decisive measurement for critical, low levels of Cr, Ni and Cu, it is necessary to grind the inspected component with an aluminum oxide disc to remove at least 0.004 inches of the surface prior to testing. Elbows, tees, reducers, couplings, flanges, welds, caps, plugs and other fittings, as well as pipe-scale can all be tested for the maximum allowable value of the sum of the three key residuals.

Model: DP-2000 (High Count Rate)
Measured values of residual elements Test time (mode): 120 Seconds B1 (Alloy Plus)
(Average of 5 repeat tests)
CrNiCu
Standard Cr Assay Cr +/- Ni Assay Ni +/- Cu Assay Cu +/-
ARMI 229A 0.015 0.01328 0.001838478 0.029 0.02858 0.002800143 0.014 0.00946 0.001555635
ARMI 28E 0.079 0.07768 0.002130748 0.145 0.14036 0.003903229 0.12 0.11628 0.00315841
ARMI 33D 0.139 0.13562 0.002545584 1.78 1.77232 0.011181715 0.072 0.07394 0.003526106
ARMI 35F 1.16 1.1579 0.005694567 0.047 0.04812 0.002988705 0.03 0.02768 0.002017611

Residual sums (Pass if <0.075%)
Results
Sample Sum of res. Inspection P/F
ARMI 229A 0.051 PASS
ARMI 28E 0.334 FAIL
ARMI 33D 1.982 FAIL
ARMI 35F 1.234 FAIL

trace cr xrf chart

Conclusion

The DELTA XRF analyzer is an essential tool for all businesses involved in the trade or use of metals alloys. In seconds, you can nondestructively measure over 25 elements. Turnings, shavings, rods, wires, small parts, components, sizeable materials and large structures can all be analyzed directly, non-destructively. Whether you check purity, chemistry, or grade ID for highest value, maximum recovery, quality, conformance, or maintenance and safety, the Olympus DELTA XRF analyzer will give you immediate answers to take preventative action.


Delta HandHeld XRF testing for alloys
Olympus IMS

Produits utilisés pour cette application
Les analyseurs XRF à main DELTA pour les applications d’identification positive des matériaux (PMI) permettent l’analyse non destructive d’alliage afin de déterminer rapidement et précisément les nuances d’alliage et la composition chimique des métaux. L’analyse et l’identification des éléments chimiques des alliages s’effectuent en quelques secondes, du simple tri lors d’applications de séparation des nuances difficiles au contrôle des matériaux entrant et jusqu’à la vérification du produit final.
Le DELTA Element est un analyseur portable par fluorescence X (XRF) économique optimisé pour le tri de la ferraille, l’identification positive des matériaux (PMI), le contrôle qualité des alliages et l’analyse des métaux précieux.
Muni d’un tube à rayons X optimisé de 4 W et d’un détecteur SDD (Silicon Drift Detector), le DELTA Professionnal offre un rendement inégalé en termes de vitesse, de limites de détection ou de gamme d’éléments. Il permet l’analyse du Mg et des éléments suivants dans les alliages et le minerai. Le DELTA Professionnal constitue la solution par excellence d’Olympus en matière d’appareil à main pour l’analyse XRF.
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.
Sorry, this page is not available in your country