Inspecting the Brazed Joints of Radiator Fins Using a Digital Microscope


Radiator fin for vehicles
Radiator fin for vehicles

Manufacturing Radiators for Vehicles

A cooling system is installed near a vehicle’s engine to keep it cool. It generally cools the engine with liquid coolant. The engine heats up the coolant, which travels through the many pipes making up the radiator where the heat is dissipated into the air. The coolant then returns to the engine, and the process repeats. The pipes in the radiator connect to fins that form a heat sink and increase cooling efficiency.

Radiators are usually made of an aluminum alloy since they have a high cooling effect. Their components are thin to expand the cooling area. The radiator pipes and fins are joined by brazing, a method of joining metal components using a melted filler metal.

There are many metal types used as the brazing filler metal, but they need to have a lower melting point than the base material to ensure that the components are not damaged during the brazing process. The filler metal joins components by flowing into the joint between the two components using the capillary effect. Brazed joints are strong and corrosion resistant, and brazing enables multiple points to be joined at once. Brazing is an effective joining method for radiator fins when multiple points need to be joined.

The Importance of Inspecting Brazed Joints

For quality control, it is important to confirm that components are brazed correctly to prevent them coming loose. If the fin separates from the joint with the pipes, it can pierce the pipes and cause a leak, which can lead to the engine overheating.

For this reason, inspectors check the brazed joint’s condition using microscopes. However, there are various microscope observation methods available, and inexperienced inspectors may have difficulty choosing an appropriate one.

Advantages of Inspecting Brazed Joints of Radiator Fins Using the DSX1000 Digital Microscope

1) Easily select the appropriate observation method with the multi-preview function

The DSX1000 microscope’s multi-preview function makes it simple to view the sample using multiple observation methods to find the right one. The microscope automatically optimizes the field stop and illumination adjustment for each observation method. This feature also helps ensure that the observations are carried out in a repeatable way regardless of operator.

Checking the observation method using the multi-preview function
Checking the observation method using the multi-preview function

Brightfield observation image, Brightfield image with upgraded contrast

The brazed joint condition is more clearly visible in the brightfield image with upgraded contrast than in the brightfield image.

2) See the details with a wide range of magnifications.

After identifying the point you want to inspect, you can quickly change the magnification using the easy-to-use optical zoom dial.

OPTICAL ZOOM
The optical zoom of up to 10X is controlled by turning the jog dial on the console box.

Front lens, Rear lens, Slide the lens to quickly change magnification

Sometimes finding the proper magnification requires you to change the objective lens. The DSX1000 microscope makes this process simple; you can quickly change objectives by sliding them back and forth. Up to two lenses can be attached to the head at the same time.

One-step lens attachment replacement

If you have to remove the objectives and insert a new one, this is also easy. You can slide the old objective out and slide the new one into place in just a few seconds. 

300X, 700X

(Left: the radiator fin's brazed condition can be seen macroscopically. Right: the brazed condition of an individual area can be seen in more detail)

3) Instantly switch observation methods.

Easily switch observation methods by pressing a button on the console box to streamline your brazed joint inspection.
 

Console box, Button to switch observation methods

Image acquired using the differential interference contrast (DIC) observation method (700x).

Image acquired using the differential interference contrast (DIC) observation method (700X).
​The brazing filler metal penetrating the joint can be seen with a stronger contrast.


 

Olympus IMS

Produits utilisés pour cette application

Obtenez de meilleures images et de meilleurs résultats. Les microscopes numériques DSX1000 vous permettent d’analyser les défaillances avec rapidité, précision et répétabilité.

Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.
Sorry, this page is not available in your country