Measuring Fiberglass Gelcoat Thickness


This application note explains how to measure the thickness of gelcoat over fiberglass.

Overview of Fiberglass Gelcoat Thickness Inspections

Gelcoat is a hard polyester resin coating that is applied over structural fiberglass. It provides a smooth, glossy protective surface that eliminates friction and improves appearance. It is commonly used on fiberglass boat hulls and on bathroom fixtures such as sinks, tubs, and shower stalls. 

Manufacturers of fiberglass products need to measure gelcoat thickness to confirm that it is within a specified range. In particular, it is important to detect where the gelcoat is too thin because of insufficient application or shrinkage. Measurements typically involve a range of about 0.25 to 1 mm (0.01 to 0.04 in.), with most cases involving a nominal thickness of around 0.5 mm (0.02 in.)

Gelcoat Thickness Gauging Equipment

Gelcoat thickness can be measured with our precision thickness gauges, such as the 39DL PLUS™ and 45MG gauges with the Single Element software option. The waveform display that is standard on the 39DL PLUS gauge and available on the 45MG gauge as an option is useful for establishing echo quality and verifying readings.

Gelcoat is normally measured with a delay line transducer. The most commonly recommended transducer is the M208-RM (20 MHz, 0.125 in. element diameter). In cases involving thick gelcoat, the M202-RM transducer (10 MHz, 0.25 in. element diameter) can also be used.

Procedure to Measure Gelcoat Thickness on Fiberglass

This application is set up as a Mode 2 measurement (interface echo to first backwall echo). The primary challenge is that the inside surface of gelcoat is usually rough and irregular, conforming to the surface profile of the fiberglass. Due to this nonuniform geometry, the quality of the echo from the gelcoat/fiberglass boundary often varies widely from point to point. The first echo from that boundary may not be the largest and phase distortion may appear to invert echoes. In some cases, roughness may drop reflected echo amplitude below the detectable minimum. Also, the gelcoat/fiberglass boundary echo is usually followed by several other peaks representing scatter noise from within the underlying fiberglass, which if detected will cause erroneously high readings.

Because manufacturers are usually most concerned about confirming that gelcoat meets a minimum thickness specification, the recommended procedure is to make several readings within a small area and record the minimum reading obtained. If a waveform display is available, then it is possible to verify whether the first returning echo (representing minimum gelcoat thickness) is being detected by monitoring the waveform display as seen in the screen images below. 

If a 45MG gauge is used without the waveform display option, it is particularly important to note the minimum reading within a local area. Any abrupt transition to a higher reading usually represents false detection caused by irregular echoes. As a general rule, the gauge gain should be set high to maximize the likelihood of detecting the first returning echo. The First Peak detection mode that is available on most of our gauge models is also useful in this application to help ensure measurement of minimum thickness.
 

Example of an optimal gelcoat reading. The first peak is detected.

Example of an optimal gelcoat reading. The first peak is detected.
 

Example of an inaccurate reading. The first peak is undetected due to low amplitude related to inside surface roughness.

Example of an inaccurate reading. The first peak is undetected due to low amplitude related to inside surface roughness.
 

Measuring Total Fiberglass Thickness

In many cases, the same gauge that is used for gelcoat measurement can also be used to measure total wall thickness (gelcoat plus fiberglass) using a second transducer, usually an M1036 (2.25 MHz, 0.5 in. element diameter, high sensitivity). The maximum measurable fiberglass thickness is typically about 12.5 mm (0.5 in.). For thicker fiberglass, a high-penetration (HP) gauge is usually required.
 

Olympus IMS

Products Used for This Application

The 39DL PLUS™ gauge is field-proven and reliable for virtually every ultrasonic thickness inspection. It works as a precision or corrosion thickness gauge to meet the challenges of demanding applications across industries, including maintenance, manufacturing, and energy production. With world-class ultrasonic capability, fast scanning speeds, and fully integrated wireless connectivity, this handheld gauge delivers results you can trust in a seamless workflow.

The 72DL PLUS™ advanced ultrasonic thickness gauge delivers precision thickness measurements at high speed in a portable, easy-to-use device. Compatible with single element transducers up to 125 MHz, this innovative instrument is ideally suited to measure the thickness of ultra-thin materials, including multilayer paint, coatings, and plastic. It can simultaneously display the thickness of up to 6 layers.

The handheld 45MG ultrasonic thickness gauge is packed with measurement features and software options. This unique instrument is compatible with the complete range of Olympus dual element and single element transducers, making this gauge an all-in-one solution for virtually every thickness gauge application.
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.
Sorry, this page is not available in your country