5CC25-32-42.3X6-R4-P-2.5-OM

5CC25-32-42.3X6-R4-P-2.5-OM

Standard Phased Array Probe, 5.0 MHz Concave in Azimuth Array 25 mm Radius, 32 Elements, 42.3x6 mm Total Active Aperture, 1.32 mm Pitch, 6 mm Elevation, R4 Case Type, Impedance Matching to Water/Aqualene, PVC Sheathing, 2.5 m Cable Length, Omniscan Connector
Item NumberPart CodeFrequency
(MHz)
Number of ElementsAngle (°)Case TypePitch (mm)Elevation (mm)Radius (mm)Estimated ship*Price
(USD)
Add to Cart
U83304795CC25-32-42.3X6-R4-P-2.5-OM53290°R41.32625

* Product lead times vary. You will receive shipping confirmation 1-2 business days after placing your order.
If you need a product sooner, please contact a sales representative for more details.


Web Store not Available

The Olympus web store is currently not available in your country. Please contact your local sales representative for further product information and purchases.

Sorry, this page is not available in your country