Here's the Dirt on Using XRD Technology to Identify the Origin of Soils

By -
Mineralogical analysis

Jose Brum, one of our XRD Applications Scientists, took part in publishing a paper and presentation in cooperation with Virginia Commonwealth University.

The researchers conducted a geochemical analysis to understand the differences in the characteristics between the soils in Meherrin, Virginia and the nearby soils of the Virginia Piedmont Region.

X-ray diffraction (XRD) analysis of separated magnetic particles was conducted using an Olympus TERRA® XRD instrument with a cobalt anode X-ray tube. The results are indicative of a possible extraterrestrial or volcanic source of iron-enriched mineral phases.

Check out the presentation:

Posted with permission from Virginia Commonwealth University.

You can also read the conference abstract.

The battery-powered TERRA XRD analyzer in the field.
The battery-powered TERRA XRD analyzer in the field.

Related Content

XRD Technology is Helping Users Who Have a Flare for Fireworks Safety

Using Portable XRD to Analyze Explosives, Forensics, and Narcotics

Out of this World: Olympus XRD on Mars

Marketing Specialist, Analytical Instruments

Michelle has more than 9 years experience in marketing communications and works in Olympus' Analytical Instruments business to promote X-ray fluorescence and X-ray diffraction analyzers. She works with product, engineering, and applications groups for new product launches, to create webinars, and to write application notes.
InSight Blogの登録

当社のブログをご覧いただき、ありがとうございます。

新しいテクノロジー、アプリケーション、いろいろなヒントやコツ、イベント情報など盛りだくさんのストーリーを、Insightで定期的に読むことができます。 ブログの内容についてご提案がありますか。私たちにお聞かせください

このページはお住まいの地域ではご覧いただくことはできません。
Let us know what you're looking for by filling out the form below.
このページはお住まいの地域ではご覧いただくことはできません。