Portable XRF and XRD at the Mine Site


Portable X-ray fluorescence (pXRF) and X-ray diffraction (pXRD) analyzers can provide significant cost and operational benefits to active mining operations. Many decisions must be made at the mine site based on geochemical and mineralogical analysis of a wide variety of sample types. pXRF and pXRD can improve the forecasting of many important rock parameters such as grade, hardness, alteration, and lithology that all impact the recovery of the economic metals being mined. These analyzers play a key role in decision-making and help optimize operational efficiency in many ways, including underground mining, open-pit mining, the production process, the laboratory, and environmental applications.

Improve the Efficiency of Your Mining Operation

  • Accurately and rapidly define ore/waste boundaries from blast holes and underground face, drive, and blast samples
  • Understand the geochemical and mineralogical dimensional characteristics of the deposit
  • Prevent problematic materials (arsenic, talc, or clay rich) from going to the mill
  • Reduce lead time associated with grade control sample analysis
  • Increase sampling numbers/density within the grade control envelope
  • Reduce mine site analytical costs and reduce the load of the mine site laboratory
  • Improve blending strategies with real-time analysis of run-of-mine (ROM) material
  • Optimize milling and crushing residence times based on analysis of silicon (Si) as a proxy for quartz

Improve Recovery of Minerals

  • Analyze feeds and tailings to optimize flow sheet
  • Understand the presence of floating clays in feeds and mid cons
  • QA/QC on concentrates
  • Copper (Cu) in liquids in solvent extraction-electrowinning (SX/EW) operations
  • Analyze arsenic (As) to inform cyanide leach specifications
  • Sulfur (S) analysis in feed to inform sulfide/oxide ratios
  • Inform flux adjustments and penalty elements in precipitates and bullion
  • Analyze smelted material for process control
  • Gold (Au) and calcium (Ca) in activated carbon
  • Uranium (U) of in-situ leaching (ISL) liquids

Easy Quantification Using XRF

  • Reduce reliance on wet chemical techniques
  • Reduce load on limited laboratory resources (time and equipment)
  • Reduce analytical turnaround time from hours to minutes
  • Baseline mine site environmental monitoring and sulfur (S) in waste rock to predict acid mine drainage (AMD)
  • Cost savings associated with reduction in lab technician times and reagents used
  • Improved safety through less use of hydrofluoric and nitric acids: reduction in skin burns and lead fumes associated with the fire assay process

Types of Mines Using Olympus pXRF and pXRD for Grade Control

  • Base metals: copper (Cu), lead (Pb), zinc (Zn), nickel (Ni), tin (Sn), tungsten (W), molybdenum (Mo), tantalum (Ta), antimony (Sb), manganese (Mn), chromium (Cr), niobium (Nb), cobalt (Co)
  • Bulk commodities: iron ore, phosphate, bauxite, coal
  • Mineral sands: titanium (Ti) and zirconium (Zr)
  • While not the primary tool for grade control, pXRF and pXRD are used extensively in gold (Au) and silver (Ag) mining and lithium (Li) production

Quantifying Copper Grade and Mineralogy Using Olympus pXRF and pXRD

(Figure 1). Analysis of grade control pulp samples from an active Cu mine using pXRF

(Figure 2). pXRD analysis of ore showing similar copper concentrations (chalcopyrite) but appreciably more chlorite, which will negatively impact the flotation process


Benefits of Vanta™ XRF Analyzers

Vanta handheld XRF analyzers enable you to analyze a range of materials quickly and nondestructively at the mine site. Benefits include:

  • Continuous operation at high temperatures: Up to 50°C (122°F)
  • IP55/IP54 rated: Withstands dirt, dust, and rain to protect against hazards in challenging environments
  • Drop tested (MIL-STD-810G): Protects against falls and reduces the need for costly repairs
  • Cloud-technology enabled: Access and share data across multiple platforms from any location

Vanta XRF

BTX III | TERRA II

Benefits of BTX™ III and TERRA™ II pXRD

  • Small Sample: Requires only 15 mg of sample
  • Easy Sample Preparation: Does not require a skilled technician
  • Fast Acquisition Time: Obtain results in only a few minutes
  • Stand-Alone Instrument: No need for water cooling or a large, external power source
  • No Ongoing Service Requirements: XRD can be performed regularly with minimal downtime
  • Portable: Battery-operated, rugged design with no moving parts
Olympus IMS

이 애플리케이션에 사용되는 제품
Vanta™ 휴대용 XRF 분석기 시리즈는 최신의 가장 강력한 휴대용 XRF 장치로서 현장에서 실험실 품질의 결과를 요구하는 고객을 위해 신속하고 정확한 요소 분석을 제공합니다. 분석기는 IP55 또는 IP54 등급으로 견고하게 제작됐으며, 가동 시간 향상과 소유 비용 절감을 위해 낙하 시험을 거쳤습니다.
TERRA™ II XRD 분석기는 휴대용 정량 광물학을 제공합니다. 최대 6시간의 배터리 수명과 견고하고 비바람을 견디는 케이스를 갖춘 이 시스템은 주요 구성품과 부속 구성품을 신속하게 현장 분석하도록 설계됐습니다.
BTX ™ III XRD 분석기는 컴팩트한 벤치탑 설계에서 주요 및 미량 성분에 대해 신뢰할 수 있는 정량적 광물학을 제공합니다. 강력한 소프트웨어는 향상된 X선 탐상기와 결합되어 속도와 감도를 향상시킵니다.
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.
아래 양식을 작성하여 원하는 내용을 알려주십시오.
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.