Dillon McDowell, one of our X-ray fluorescence (XRF) Applications Scientists, presented a paper at the 15th Asia Pacific Conference for Nondestructive Testing (APCNDT 2017) in Singapore.

Dillon’s paper, “Screening of Ceramic and Leaded Contaminants in Glass Recycling Streams via Handheld X-ray Fluorescence (HHXRF) Analyzers” was coauthored with Olympus Applications Manager, Alex Thurston.

In the paper, Dillon discusses the techniques, drawbacks, and benefits of recycling glass and ceramic glass. One challenge that material recovery facilities (MRFs) face is that the magnetic and optical sorting systems they normally use to separate glass cullet from recycled glass are not effective at screening glass ceramic and leaded constituents from cullet streams. These contaminants lower the value of glass cullet to glass manufacturers. Handheld X-ray fluorescence analyzers are widely used since they can provide material chemistry results quickly. The results of this study demonstrate that HHXRF can detect even small quantities of ceramic elements in glass and glass cullet and that lead and color agents (iron (Fe) and copper (Cu)) can be reliably detected within seconds. Dillon also demonstrates that in-line XRF systems can be adapted to provide fast, reliable results that can keep up with the speed that cullet is typically measured.

Check out the presentation


Get In Touch
마케팅 전문가, 분석 장비

Michelle은 마케팅 커뮤니케이션에 9년 이상의 경력을 가지고 있으며, Olympus의 분석 장비 사업에서 X선 형광 및 X선 회절 분석기를 담당하고 있습니다. 그녀는 신제품 출시를 위해 제품, 엔지니어링 및 학술 지원 그룹과 협력하여 웨비나를 제작하고 애플리케이션 노트를 작성합니다.

3월 14, 2018
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.
InSight 블로그 가입하기
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.
아래 양식을 작성하여 원하는 내용을 알려주십시오.
죄송합니다. 이 페이지는 해당 국가에서 사용할 수 없습니다.