OLYMPUS LCPLFLN-LCD 렌즈는 LCD 패널등의 유리기판을 통하여 내부관찰을 할 수 있는 최적의 렌즈입니다. Optical Correction Rings 을 사용하여 유리두께에 따른 색수차를 보정할 수 있습니다. | ![]() |
Magnification [X] | 20 |
---|---|
Numerical aperture (NA) | 0.45 |
Working distance (WD) [mm] | 7.40 - 8.30 |
Objective Field Number | 26.5 |
Immersion medium | Air/Dry |
Spring loaded | N/A |
Correction collar | Yes |
Correction range of correction collar | Glass: 0 - 1.2mm |
Iris | N/A |
Correction level of chromatic aberration |
Semi-apochromat
(FL) |
Parfocalizing distance [mm] | 45 |
Back focal plane (BFP) position | -3.0 |
Type of screw thread | W20.32X0.706(RMS) |
Brightfield(Reflected) | Good |
Brightfield(Transmitted) | Good |
Darkfield(Reflected) | N/A |
Darkfield(Transmitted) | N/A |
DIC(Reflected) | Limitation |
DIC(Transmitted) | N/A |
Phase Contrast | N/A |
Relief Contrast | N/A |
Polarized Light | N/A |
Fluorescence (B, G Excitation) | N/A |
UV Fluorescence (at 365nm) | N/A |
Multiphoton | N/A |
TIRF | N/A |
IR | N/A |
WLI | N/A |
Auto Focus | N/A |
*Value at glass thickness 0.7mm observation
Magnification [X] | 50 |
---|---|
Numerical aperture (NA) | 0.7 |
Working distance (WD) [mm] | 2.20 - 3.00 |
Objective Field Number | 26.5 |
Immersion medium | Air/Dry |
Spring loaded | N/A |
Correction collar | Yes |
Correction range of correction collar | Glass: 0 - 1.2mm |
Iris | N/A |
Correction level of chromatic aberration | Semi-apochromat |
Parfocalizing distance [mm] | 45 |
Back focal plane (BFP) position | -3.0 |
Type of screw thread | W20.32X0.706(RMS) |
Brightfield(Reflected) | Good |
Brightfield(Transmitted) | Good |
Darkfield(Reflected) | N/A |
Darkfield(Transmitted) | N/A |
DIC(Reflected) | Limitation |
DIC(Transmitted) | N/A |
Phase Contrast | N/A |
Relief Contrast | N/A |
Polarized Light | N/A |
Fluorescence (B, G Excitation) | N/A |
UV Fluorescence (at 365nm) | N/A |
Multiphoton | N/A |
TIRF | N/A |
IR | N/A |
WLI | N/A |
Auto Focus | N/A |
*Value at glass thickness 0.7mm observation
Magnification [X] | 100 |
---|---|
Numerical aperture (NA) | 0.85 |
Working distance (WD) [mm] | 0.90 - 1.20 |
Objective Field Number | 26.5 |
Immersion medium | Air/Dry |
Spring loaded | N/A |
Correction collar | Yes |
Correction range of correction collar | Glass: 0 - 0.7mm |
Iris | N/A |
Correction level of chromatic aberration | Semi-apochromat(FL) |
Parfocalizing distance [mm] | 45 |
Back focal plane (BFP) position | -3.0 |
Type of screw thread | W20.32X0.706(RMS) |
Brightfield(Reflected) | Good |
Brightfield(Transmitted) | Good |
Darkfield(Reflected) | N/A |
Darkfield(Transmitted) | N/A |
DIC(Reflected) | Limitation |
DIC(Transmitted) | N/A |
Phase Contrast | N/A |
Relief Contrast | N/A |
Polarized Light | N/A |
Fluorescence (B, G Excitation) | N/A |
UV Fluorescence (at 365nm) | N/A |
Multiphoton | N/A |
TIRF | N/A |
IR | N/A |
WLI | N/A |
Auto Focus | N/A |
*Value at glass thickness 0.7mm observation
You are being redirected to our local site.