Thickness Measurements on Rubber Sheets and Coatings
Rubber sheets and coatings can be difficult to gauge with conventional mechanical thickness measurement techniques. However, ultrasonic thickness gauging enables measurements on any point on the surface of a rubber sheet—not just the edges—without contacting the opposite side. Ultrasound waves travel through the rubber coating and reflect from the acoustic interface of the rubber and the substrate. This acoustic interface can be air, rubber steel, rubber composite, or other
materials as long as the outside surface of the rubber is available for probe coupling.
It is important to fully understand the application before taking thickness measurements. Rubber coating on certain materials may require special setups to maintain accurate thickness readings.
Ultrasonic Equipment Used for Thickness Measurements on Rubber Sheets
Ultrasonic thickness measurements on rubber sheets can be performed using precision thickness gauges, such as the 39DL PLUS™ gauge and the 45MG gauge with Single Element software. When combined with the appropriate transducers between 2.25 MHz and 20 MHz, these handheld gauges can typically measure rubber materials in the range of 0.008 to 0.250 in. (0.2 to 6 mm). This range will vary depending on
the transducer and setup being used. Thick or attenuating rubber materials will require the High Penetration software option for the 39DL PLUS and 45MG gauges.
The 72DL PLUS™ gauge offers a larger touch-screen display and a higher measurement update rate (up to 2 KHz). This gauge is available in a high-frequency version (up to 125 MHz) for measuring very thin rubber coatings. It can measure much thinner materials than conventional ultrasonic thickness gauges.
The 39DL PLUS™ gauge is field-proven and reliable for virtually every ultrasonic thickness inspection. It works as a precision or corrosion thickness gauge to meet the challenges of demanding applications across industries, including maintenance, manufacturing, and energy production. With world-class ultrasonic capability, fast scanning speeds, and fully integrated wireless connectivity, this handheld gauge delivers results you can trust in a seamless workflow.
The 72DL PLUS™ advanced ultrasonic thickness gauge delivers precision thickness measurements at high speed in a portable, easy-to-use device. Compatible with single element transducers up to 125 MHz, this innovative instrument is ideally suited to measure the thickness of ultra-thin materials, including multilayer paint, coatings, and plastic. It can simultaneously display the thickness of up to 6 layers.
Zaawansowany grubościomierz ultradźwiękowy 45MG dostępny jest ze standardowymi funkcjami pomiarowymi oraz z opcjami oprogramowania. Ten unikalny przyrząd jest kompatybilny z całą gamą głowic jedno- i dwuprzetwornikowych do pomiaru grubości firmy Olympus.
Grubościomierz z czujnikiem hallotronowym Magna-Mike™ jest wyposażony w sondę magnetyczną umożliwiającą wykonywanie dokładnych pomiarów materiałów nieżelaznych i cienkich, takich jak butelki z tworzywa sztucznego.
Sorry, this page is not available in your country
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.