Thickness Testing of Reinforced Rubber Conveyor Belts


m1036 testing thinkness of rubberThis application note explores how to measure the depth of textile and steel reinforcements in rubber conveyor belts, as well as measure the remaining rubber thickness of in-service belts during maintenance. 

Background on Conveyor Belt Manufacturing

A wide variety of rubber conveyor belts for heavy-duty industrial and mining services, such as ore and mineral transportation, incorporate internal layers of woven fabric or steel cords for strength reinforcement. Conveyor belt manufacturers need to check the depth of the reinforcement layer across the belt to confirm that the product meets specification. After installation, belt users need to periodically check the thickness of the remaining rubber as the belt wears down to estimate the remaining service life before replacement. Large belts can be expensive, so accurate information on remaining rubber thickness is valuable to users. Our instruments and transducers have been successfully employed in this test for many years.

Sound energy reflects off the first layer of reinforcement. In the case of textile or fabric reinforced belts, very little sound energy will penetrate deeper. Measurement of total belt thickness is normally possible only in the case of some steel-reinforced belts where there is sufficiently wide separation between the steel cords to permit sound energy to travel unobstructed to the opposite side of the belt. However, the critical dimension for most users is the amount of rubber over the first reinforcement layer, not total thickness. This is usually a straightforward application for ultrasonic thickness gauging.

Ultrasonic Equipment for Measuring Conveyor Belt Rubber Thickness

Conveyor belt rubber thicknesses under approximately 12.5 mm or 0.5 in. can usually be measured with standard thickness gauge models, such as the 39DL PLUS™ gauge or 45MG gauge with Single Element software. For greater thicknesses, use the High Penetration software option for these gauges. Thickness measurements can also be made with any of the EPOCH™ series ultrasonic flaw detectors. In the case of certain very large belts, with rubber thicknesses approaching 50 mm or 2 in., the EPOCH flaw detectors are the preferred instruments.

The transducer selection will depend on the range of rubber thickness to be measured. For rubber layers between approximately 1 mm (0.040 in.) and 6.25 mm (0.250 in.), a 2.25 MHz delay line transducer (M207-RB) is usually recommended. For measurement of rubber between approximately 2.5 mm (0.1 in.) and 25 mm (1 in.), a 2.25 MHz high penetration contact transducer (M1036) is commonly used. Other transducers are available for thinner and thicker rubber layers.

As with any application involving attenuating materials, using gel couplant or glycerin (Couplant B) is recommended in preference to less viscous fluids. For severely worn in-service belts, remove any loose rubber or other debris from the surface before testing.

Ultrasonic Gauging Procedure to Measure Conveyor Belt Thickness

In the most common situation using the M1036 transducer to measure the outer rubber layers on belts with textile or fabric reinforcement, start with the gauge's M1036 default setup and increase maximum gain as necessary to measure the thickness range of interest. If necessary for measurement of thin belts, increase initial gain as well. In any of these setups, gain may usually be increased up to the point where the gauge displays a constant false reading when the transducer is uncoupled, which indicates that gain is too high.

measurement with M1036

Typical conveyor belt measurement with an M1036 transducer

To measure thin rubber layers over textile or fabric reinforcement with the M207 delay line transducer, use the M207 Mode 2 default setup and adjust gain and blanking as necessary based on the echoes from a reference standard.



measurement with M207

Typical thin rubber layer measurement with an M207 transducer

Measurement of depth of braided steel cord reinforcements can be more challenging because their irregular contour presents a less optimum reflecting surface. Careful adjustment of instrument gain with the aid of a reference sample is recommended. Also note that echo polarity will be positive rather than negative because the steel represents a high impedance reflector.

measurement with M1036

Steel cord depth measurement with M1036

Sound velocity in rubber compounds will typically be on the order of 1.650 mm/µS or 0.0650 in/µS. The Olympus Applications Lab is always available to assist with gage setups for specific transducers and belt types.

Olympus IMS

ProductsUsedApplications

The 39DL PLUS™ gauge is field-proven and reliable for virtually every ultrasonic thickness inspection. It works as a precision or corrosion thickness gauge to meet the challenges of demanding applications across industries, including maintenance, manufacturing, and energy production. With world-class ultrasonic capability, fast scanning speeds, and fully integrated wireless connectivity, this handheld gauge delivers results you can trust in a seamless workflow.

The 72DL PLUS™ advanced ultrasonic thickness gauge delivers precision thickness measurements at high speed in a portable, easy-to-use device. Compatible with single element transducers up to 125 MHz, this innovative instrument is ideally suited to measure the thickness of ultra-thin materials, including multilayer paint, coatings, and plastic. It can simultaneously display the thickness of up to 6 layers.

The EPOCH 650 is a conventional ultrasonic flaw detector with excellent inspection performance and usability for a wide variety of applications. This intuitive, rugged instrument is a continuation of the popular EPOCH 600 flaw detector with additional capabilities.
Zaawansowany grubościomierz ultradźwiękowy 45MG dostępny jest ze standardowymi funkcjami pomiarowymi oraz z opcjami oprogramowania. Ten unikalny przyrząd jest kompatybilny z całą gamą głowic jedno- i dwuprzetwornikowych do pomiaru grubości firmy Olympus.
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.
Sorry, this page is not available in your country