Ring/Donut, or encircling probes are made to fit various fastener head diameters. They are mainly used for subsurface crack detection with the fastener in place. They are available in both bridge and reflection configurations. Advantages
| ![]() |
Coil | Frequency | ID mm (in.) | OD mm (in.) | Connector | Part ID | U8 # | Cable | Item # |
Bridge | 50 Hz to 500 Hz | 8.89 (0.35) | 19.05 (0.75) | Triax Fischer | LR017-5-TF | U8636097 | 9122244 | U8800091 |
Bridge | 50 Hz to 500 Hz | 17.8 (0.7) | 33 (1.3) | Microdot | LR0113-5 | U8636094 | 9102894 | U8800041 |
Bridge | 50 Hz to 500 Hz | 19.05 (0.75) | 32.5 (1.28) | Microdot | LR0114-5 | U8636071 | 9102894 | U8800041 |
Bridge | 50 Hz to 500 Hz | 19.05 (0.75) | 32.5 (1.28) | Triax Fischer | LR0114-5-TF | U8636072 | 9122244 | U8800091 |
Bridge | 500 Hz to 10 kHz | 6.48 (0.255) | 16.51 (0.65) | Microdot | LR106-1 | U8636107 | 9102894 | U8800041 |
Bridge | 500 Hz to 10 kHz | 6.48 (0.255) | 16.51 (0.65) | Triax Fischer | LR106-1-TF | U8620455 | 9122244 | U8800091 |
Bridge | 500 Hz to 10 kHz | 7.62 (0.3) | 19.05 (0.75) | Triax Fischer | LR107-1-TF | U8636077 | 9122244 | U8800091 |
Bridge | 3 kHz to 20 kHz | 7.99 (0.315) | 17.2 (0.68) | Triax Fischer | LR506-2 | U8620265 | 9122244 | U8800091 |
Bridge | 50 Hz to 500 Hz | 25.4 (1.0) | 38.35 (1.51) | Microdot | LR0115-1 | U8636095 | 9102894 | U8800041 |
Bridge | 300 Hz to 5 kHz | 12.7 (0.5) | 25.4 (1.0) | Triax Fischer | LR0510-5-TF | U8636098 | 9122244 | U8800091 |
Bridge | 300 Hz to 5 kHz | 7.62 (0.3) | 19.81 (0.78) | Triax Fischer | LR058-1-TF | U8636089 | 9122244 | U8800091 |