Defektoskopy
Accupath & Short Approach Wedges
Accupath Wedges
- Small wedge footprint
- Pointed toe design allows transducer rotation even when the nose is touching a weld crown
- Special wedge design for use with 10 MHz transducer
| ![](https://static1.olympus-ims.com/data/Image/panaCat/il/wedgeTransducers%20Graphic.jpg?rev=976E) |
Accupath and Surface Wave Wedge Dimensions* (Miniature Screw-in) |
Fits Nominal Element Size (in inches)
|
| |
0.5
| |
0.375
| |
0.25
|
| |
(A)
|
(B)
|
(C)
|
(D)
| |
(A)
|
(B)
|
(C)
|
(D)
| |
(A)
|
(B)
|
(C)
|
(D)
|
30°
| |
0.72
|
1.22
|
0.77
|
0.54
| |
0.62
|
1.03
|
1.03
|
0.42
| |
0.49
|
0.66
|
0.45
|
0.23
|
45°
| |
0.70
|
1.03
|
0.73
|
0.38
| |
0.60
|
0.85
|
0.61
|
0.32
| |
0.43
|
0.61
|
0.43
|
0.235
|
60°
| |
0.74
|
1.19
|
0.73
|
0.45
| |
0.67
|
1.00
|
0.61
|
0.367
| |
0.48
|
0.71
|
0.43
|
0.268
|
70°
| |
0.79
|
1.34
|
0.73
|
0.50
| |
0.69
|
1.12
|
0.61
|
0.406
| |
0.50
|
0.81
|
0.43
|
0.305
|
90°
| |
1.25
|
1.84
|
0.77
|
-
| |
1.00
|
1.48
|
1.48
|
-
| |
0.83
|
1.13
|
0.45
|
-
|
Miniature Screw-In Wedges for 10 MHz Transducers
Nominal Element Size
|
Wedge Part Numbers
|
inches
|
mm
|
Accupath*
|
Surface Wave 90°
|
0.50
|
13
|
ABWM-5ST-X°
|
ABWML-5ST-90°
|
0.375
|
10
|
ABWM-7ST-X°
|
ABWML-7ST-90°
|
0.25
|
6
|
ABWM-4ST-X°
|
ABWML-4ST-90°
|
*Accupath Wedges are available in standard refracted shear wave angles of 30°, 45°, 60°, and 70° in steel at 10 MHz.
Short Approach Wedges
- Smallest footprint
- Short approach distance allows for inspection closest to the weld crown
| ![](https://static2.olympus-ims.com/modules/imageresizer/006/a00/0422f9d769/125x98p108x85.jpg) |
Short Approach Wedge Dimensions (Miniature Screw-in)
|
Fits Nominal Element Size (in inches)
|
|
0.5
|
0.375
|
0.25
|
|
(A)
|
(B)
|
(C)
|
(D)
|
(A)
|
(B)
|
(C)
|
(D)
|
(A)
|
(B)
|
(C)
|
(D)
|
45°
|
0.70
|
1.03
|
0.73
|
0.38
|
0.60
|
0.85
|
0.61
|
0.32
|
0.43
|
0.61
|
0.43
|
0.235
|
60°
|
0.74
|
1.19
|
0.73
|
0.45
|
0.67
|
1.00
|
0.61
|
0.367
|
0.48
|
0.71
|
0.43
|
0.268
|
70°
|
0.79
|
1.34
|
0.73
|
0.50
|
0.69
|
1.12
|
0.61
|
0.406
|
0.50
|
0.81
|
0.43
|
0.305
|
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.
Redirecting
You are being redirected to our local site.
Sorry, this page is not available in your country