Evident LogoOlympus Logo
Resources
Application Notes
Back to Resources

Portable XRD for Lithium


Exploration, Mining, and Extraction in Pegmatite Deposits

Olympus portable X-ray diffractometers (pXRD), such as the TERRA® analyzer, provide geologists and metallurgists with quantitative mineralogy in near real time, across all mineral species. Exploration geologists can use the TERRA analyzer to make more informed decisions in the field. Metallurgists can use pXRD to obtain the information needed to develop more effective blending strategies and optimize processing and refining techniques to yield better lithium recoveries.

Benefits of Olympus pXRD

Olympus’ innovative pXRD analyzers offer many advantages:

  • Small sample: requires only 15 mg of material
  • Easy sample preparation: does not require a skilled technician
  • Fast acquisition time: obtain results in a few minutes
  • Stand-alone instrument: no need for water cooling or a large, external power source
  • No ongoing servicing requirements: XRD can be performed regularly with minimal downtime
  • Portability: battery-operated, rugged design with no moving parts
 
Portable XRD for Lithium

Exploration

Lithium can be hosted within a range of minerals in pegmatitic rocks. A list of the main lithium-bearing minerals is provided in Table 1. Olympus pXRD can rapidly identify and quantify all these lithium-bearing minerals, irrespective of their reflectance. Quantitative mineralogy can then be back calculated to chemistry to provide geologists with excellent estimates of lithium concentrations while in the field (Figure 1). Rather than waiting days or weeks for lithium assay data from a laboratory, exploration geologists can use Olympus pXRD to make the following types of informed decisions in near real time:

  • Whether to abandon or extend a drill hole
  • Where to place the next drill hole
  • Whether to continue mapping in a specific area
Portable XRD for Lithium

Figure 1: Comparison between Li2O measured by a laboratory compared to estimates from quantitative XRD.
 
Mineral Name Li2O (%) Chemical Formula
Spodumene 8.03 LiAlSi4O6
Petalite 4.50 LiAlSi4O10
Eucryptite 11.86 LiAlSiO4
Anblygonite 7.40 (Li,Na)Al(PO4)(F,OH)
Lepidolite 7.70 K(Li,Al)3(Si,Al)4O10(F,OH)2
Lithiophilite 9.53 LiMnPO4
Zinnwaldite 3.42 KLiFeAl(AlSi3)O10(F,OH)2
Holmquistite 3.98 Li2(Mg,Fe2+)3Al2Si8O22(OH)2
Triphylite 9.47 Li(Fe,Mn)PO4

Table 1. Main Lithium-bearing minerals and chemistry (source: webmineral.com).

Processing and Extraction

Knowing Li2O concentration is important, but a knowledge of the lithium-bearing phases present (and their quantities) is often more important. Lithium can be easily extracted from some minerals yet difficult to near impossible to extract from others. With access to quantitative mineralogy, metallurgists are able to develop more appropriate blending strategies and optimize their processes accordingly.

XRD can also be used to identify gangue minerals that can downgrade lithium concentrates. For example, gravity separation is a metallurgical process that can be used to concentrate spodumene. As other non-lithium-bearing pyroxene minerals have a similar specific gravity to spodumene, it is important to identify and quantify other pyroxene minerals.

Data Quality

Portable Olympus XRD analyzers can provide data equivalent to that of laboratory XRD instruments. To illustrate this, results of quantitative XRD analysis from a lithium-bearing pegmatite were back calculated to chemistry and the results compared to laboratory chemical assay (Table 2 and Figures 1 and 2).

SiO2 Li2O Al2O3 Na2O K2O
XRD Assay XRD Assay XRD Assay XRD Assay XRD Assay
79.37 75.59 1.33 1.57 13.29 15.00 3.98 3.45 2.04 2.42
80.18 75.07 4.29 4.19 15.20 17.13 0.33 0.65

78.39 74.08 2.66 2.70 14.80 16.54 2.17 2.34 1.99 1.88
79.26 75.44 1.22 1.30 13.18 15.08 3.83 3.57 2.51 2.82
70.98 68.53 6.18 6.28 22.15 22.57 0.53 0.47 0.17 0.44
76.01 74.20 0.59 0.43 14.18 14.95

2.37 3.22
74.01 75.90 2.53 2.76 16.50 17.30

1.83 1.25
73.62 73.40 1.44 1.27 14.74 16.70

5.68 5.32
76.66 72.50 0.22 0.19 12.67 14.30

4.35 4.42
75.04 74.70 0.75 0.75 15.58 15.45

2.09 1.92


Table 2. Comparison between Si2O, Li2O, Al2O3, Na2O, and K2O measured by a laboratory compared to estimates from quantitative XRD.

Figure 2. Comparison between Al2O3, SiO2, Na2O and K2O measured by a laboratory compared to estimates from quantitative XRD.
Figure 2. Comparison between Al2O3, SiO2, Na2O and K2O measured by a laboratory compared to estimates from quantitative XRD.

Olympus IMS

ProductsUsedApplications
The TERRA Mobile XRD System, a high performing, completely contained, battery operated, closed-beam portable XRD, provides full phase ID of major, minor and trace components with a quick XRF scan of elements Ca – U. Its unique, minimal sample prep technique and sample chamber allow for fast, in-field analysis.
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.
Sorry, this page is not available in your country