The DELTA Tube Based Handheld XRF with the new, proprietary SmartScreen™ method for LBP measurements provides fast and accurate analysis of lead (Pb) in paint without radioactive isotopes.

Fast, Accurate Handheld XRF with New SmartScreen™ Method*

For LBP testing, the DELTA XRF with SmartScreen™ adjusts speed of measurement for optimum accuracy and maximum productivity. Most tests take less than 3 seconds. Even the longest tests are typically less than 10 seconds.

The absolute sensitivity for the DELTA tube based - SDD technology on surface coatings and materials, based on a 120 second test time, is 0.1μg/cm2 or 0.0001mg/cm2. Although many other conditions exist, the table below gives precision data in the context of residential Pb paint testing - where the action levels are typically in the 1.0mg/cm2 range and testing times are often less than 10 seconds.

DELTA XRF SmartScreen™ 3-σ Precision

Pb Concentration 0.3 mg/cm2 Pb in Paint
LBP Sample Type Surface Buried
(12 layers of blank paint)
3 seconds test 0.053 0.08
10 seconds test 0.03 0.04

For most paint matrices, whether positive or negative for Pb, SmartScreen™ can deliver a rapid, accurate result. However, when SmartScreen™ identifies a challenging paint matrix through spectral analysis, it extends the measurement time as required for greater accuracy and analytical confidence.

Tube Based LBP Inspections No Radioactive Isotopes

  • DELTA handheld XRF analyzers use X-ray tube sources, unlike radioactive isotope sources which are known to be slower and fade over time, requiring frequent resourcing or factory recalibrations.
  • The X-ray tube output of a DELTA remains constant for testing with the same precision and speed for its entire life; it starts fast and stays fast.
  • X-ray tube based analyzers are much less likely to report false LBP positives than radioactive isotope based analyzers when the Pb is actually in a solid structure, for example on the far side of a wall or door.
  • X-ray tube based analyzers eliminate business liabilities associated with owning hazardous radioactive isotopes.
  • DELTA handheld XRF analyzers are reliable, light-weight, and ergonomically designed. Optionally available dust wipe, filter, and soil analysis add-on capabilities can help expand business opportunities to other environmental safety inspections without having to purchase a second analyzer.
  • The overall low total cost of ownership is a benefit with the DELTA handheld XRF - no resourcing, no biannual leak tests, no radioactive disposal costs, and no increased testing time with age.

*Patent rights Protection by but not limited to US61727350

*The DELTA does not have a HUD PCS; therefore, it is not suitable for HUD LBP applications.

Olympus IMS

ProductsUsedApplications
Analisador manual por XRF Delta para teste de chumbo (Pb) em pinturas em segundos. Essas unidades confiáveis, baseadas em tubos, são leves e com design ergonômico para serem utilizadas o dia todo. Eles começam rápidas e continuam rápidas — nenhum isótopo desaparece. E elas têm uma baixo custo de propriedade. Antes de começar a manutenção estrutural — moagem, corte ou pintura — rastreie o chumbo (Pb); então, verifique a área de trabalho após a limpeza.
Juntamente com o detector de desvio de silício (SDD) e o tubo de raios X de 4W otimizado, o DELTA Professional proporciona desempenho superior em velocidade, limites de detecção e variedade de elementos. Analisa Mg e elementos superiores em ligas e mineração. O DELTA Professional é o analisador manual por XRF com melhor custo-benefício da Olympus.
Desculpe, esta página não está disponível no seu país
Diga-nos o que você está procurando preenchendo o formulário abaixo.
Desculpe, esta página não está disponível no seu país