Integral angle beam transducers provide superior signal-to-noise characteristics and contain durable plastic wear. Both Right Microdot and Straight Microdot connectors are available on some styles.
| ![]() |
![]() A592S-SM | ![]() 0.25", SM STYLE for Aluminum | ![]() A5952S-RM.tif A592S-RM | ![]() 0.25", RM STYLE for Aluminum |
*A564S-RM, A574S-RM and A5053 create surface waves in steel and aluminum.
![]() 0.187", RM STYLE | ![]() A5023 | ![]() 0.187", SM STYLE | ![]() A5014 | ![]() 0.25", RM STYLE for Steel |
Frequency (MHz) | Nominal Element Size | ACCUSCAN-S | ||||||||||||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
in. | mm | Part / Item No. | ||||||||||||||||||||||
2.25 | 0.25 x 0.25 | 6 x 6 | A561S-RM U8431041
A562S-RM U8431042
A563S-RM U8431043
A564S-RM U8431044
| |||||||||||||||||||||
5 | 0.25 x 0.25 | 6 x 6 | A591S-SM U8431052
A593S-SM U8431056
A592S-SM U8431054
A571S-RM U8431045
A572S-RM U8431046
A573S-RM U8431047
A574S-RM U8431048
A591S-RM U8431051
A592S-RM U8431053
A593S-RM U8431055
| |||||||||||||||||||||
5 | 0.187 x 0.187 | 5 x 5 | A5020 U8438003
A5021 U8438004
A5015 U8438002
A5023 U8438005
A5067 U8438014
A5068 U8438015
A5069 U8438016
A5013 U8860363
A5014 U8438001
| |||||||||||||||||||||
10 | 0.187 x 0.187 | 5 x 5 | A5054U8438012
|
Miniature potted angle beam transducers provide an excellent balance between size and performance by utilizing integral angle beam shear wave wedges. Overall size and footprint are reduced compared to a screw-in style transducer and wedge with little or no sacrifice in performance. Epoxy housings prevent test surface scratching caused by the transducer.
Connectors are available in either top (straight) or side (right angle) mount depending on application requirements. Four standard shear wave angles of 45°, 60°, 70°, and 90° or custom angles are available upon request.
![]() |
|
The sub-miniature (HS-225) and ultra-miniature (HS-877) angle beam transducers are supplied in frequencies from 2.25 to 10.0 MHz with angles from 45° through 90°. Epoxy housings prevent the transducer from causing scratches to the test surface. These transducers are ideal for inspection of small diameter welded tubes and applications where the requirement is for a shear-wave transducer with a very small footprint. Depending on the type selected, either top or side mounted, Microdot connectors are available. When ordering, please specify part number, frequency, angle, material to be inspected, and connector location.
|
Item Number | Part Code | Frequency (MHz) | Nominal Element Size | Angle (°) | Connector Type | |||
---|---|---|---|---|---|---|---|---|
mm | Inches | |||||||
U8503183
| PAB-0204-60-AL-RM | 2.25 | 6 x 6 | 0.250 x 0.250 | 60° Shear Wave in Steel | Right Microdot | ||
U8503124
| HS-225-5-45-AL-RM | 5 | 3 x 6 | 0.120 x 0.250 | 45° Shear Wave in Aluminum | Right Microdot | ||
U8503092
| PAB-0504-70-ST-RM | 5 | 6 x 6 | 0.250 x 0.250 | 70° Shear Wave in Steel | Right Microdot | ||
U8503091
| PAB-0504-70-AL-RM | 5 | 6 x 6 | 0.250 x 0.250 | 70° Shear Wave in Aluminum | Right Microdot | ||
U8503110
| PAB-0504-60-AL-SM | 5 | 6 x 6 | 0.250 x 0.250 | 60° Shear Wave in Aluminum | Straight Microdot | ||
U8430039
| PAB-0504-45-ST-RM | 5 | 6 x 6 | 0.250 x 0.250 | 45° Shear Wave in Steel | Right Microdot | ||
U8503107
| PAB-0504-45-AL-RM | 5 | 6 x 6 | 0.250 x 0.250 | 45° Shear Wave in Aluminum | Right Microdot | ||
U8435040
| HS-225-5-70-ST-RM | 5 | 3 x 6 | 0.120 x 0.250 | 70° Shear Wave in Steel | Right Microdot | ||
U8503056
| HS-225-5-70-AL-SM | 5 | 3 x 6 | 0.120 x 0.250 | 70° Shear Wave in Aluminum | Straight Microdot | ||
U8503090
| PAB-0504-60-ST-SM | 5 | 6 x 6 | 0.250 x 0.250 | 60° Shear Wave in Steel | Straight Microdot | ||
U8503163
| PAB-0504-60-ST-RM | 5 | 6 x 6 | 0.250 x 0.250 | 60° Shear Wave in Steel | Right Microdot | ||
U8503106
| PAB-0504-45-AL-SM | 5 | 6 x 6 | 0.250 x 0.250 | 45° Shear Wave in Aluminum | Straight Microdot | ||
U8503123
| HS-225-5-70-AL-RM | 5 | 3 x 6 | 0.120 x 0.250 | 70° Shear Wave in Aluminum | Right Microdot | ||
U8435041
| HS-225-5-60-ST-RM | 5 | 3 x 6 | 0.120 x 0.250 | 60° Shear Wave in Steel | Right Microdot | ||
U8503086
| PAB-0503-70-AL-SM | 5 | 5 x 5 | 0.187 x 0.187 | 70° Shear Wave in Aluminum | Straight Microdot | ||
U8503093
| PAB-0504-70-ST-SM | 5 | 6 x 6 | 0.250 x 0.250 | 70° Shear Wave in Steel | Straight Microdot | ||
U8503054
| HS-225-5-60-AL-SM | 5 | 3 x 6 | 0.120 x 0.250 | 60° Shear Wave in Aluminum | Straight Microdot | ||
U8503089
| PAB-0504-45-ST-SM | 5 | 6 x 6 | 0.250 x 0.250 | 45° Shear Wave in Steel | Straight Microdot | ||
U8503082
| PAB-0503-60-AL-SM | 5 | 5 x 5 | 0.187 x 0.187 | 60° Shear Wave in Aluminum | Straight Microdot | ||
U8503127
| HS-877-5-45-ST-RM | 5 | 5 x 5 | 0.187 x 0.187 | 45° Shear Wave in Steel | Right Microdot | ||
U8503134
| HS-225-5-45-AL-SM | 5 | 3 x 6 | 0.120 x 0.250 | 45° Shear in Aluminum | Straight Microdot | ||
U8503053
| HS-225-5-60-AL-RM | 5 | 3 x 4 | 0.120 x 0.250 | 60° Shear Wave in Aluminum | Right Microdot | ||
U8503077
| PAB-0503-45-AL-RM | 5 | 5 x 5 | 0.187 x 0.187 | 45° Shear Wave in Aluminum | Right Microdot | ||
U8503109
| PAB-0504-60-AL-RM | 5 | 6 x 6 | 0.250 x 0.250 | 60° Shear Wave in Aluminum | Straight Microdot | ||
U8503177
| PAB-1004-45-ST-RM | 10 | 6 x 6 | 0.250 x 0.250 | 45° Shear Wave in Steel | Right Microdot | ||
U8503176
| PAB-1004-45-AL-SM | 10 | 6 x 6 | 0.250 x 0.250 | 45° Shear Wave in Aluminum | Straight Microdot | ||
U8503096
| PAB-1004-45-AL-RM | 10 | 6 x 6 | 0.250 x 0.250 | 45° Shear Wall in Aluminum | Right Microdot | ||
U8502019
| PAB-1003-60-AL-SM | 10 | 5 x 5 | 0.187 x 0.187 | 60° Shear Wave in Aluminum | Straight Microdot | ||
U8503058
| HS-877-10-45-AL-SM | 10 | 3 x 4 | 0.187 x 0.187 | 45° Shear Wave in Aluminum | Straight Microdot | ||
U8503126
| HS-877-10-60-AL-SM | 10 | 5 x 5 | 0.187 x 0.187 | 60° Shear Wave in Aluminum | Straight Microdot | ||
U8503164
| HS-877-10-70-AL-SM | 10 | 5 x 5 | 0.187 x 0.187 | 70° Shear Wave in Aluminum | Straight Microdot |
You are being redirected to our local site.