Observation and measurement of profile changes in wiper blades using a laser microscope


Wiper blade
Wiper blade

Application

Automobile wiper blades are subjected to significant changes in temperature and humidity, and they are required to remain durable under severe service conditions.
Observing and measuring the wiper’s rubber blade before and after durability testing to look for the presence of tears, cracks, deformation, and the presence of foreign matter helps manufacturers design and create products that are more durable. However, it has been difficult quantitatively measure changes in the wiper’s surface profile. 

Olympus' solution

The LEXT OLS5000 microscope enables users to measure changes in the wiper’s surface profile using images and provides quantitative data.  

Product features

(1) Color and laser images and 3D profile data can be obtained at the same time, expanding the range of your analysis.
(2) By freely drawing a measurement line on the area you want to measure in the image, a cross-sectional profile can be displayed to measure the step, width, and cross-sectional area between any two points.
(3) The analysis function enables operators of any skill level to easily measure the step, line width, surface roughness, and volume by specifying the measurement region. The system continuously obtains accurate results.

​Wiper blade (Top: new wiper blade; bottom: blade after durability test)
Wiper blade (Top: new wiper blade; bottom: blade after durability test)

​Surface profile measurement of a new wiper blade; 50X objective lens
Surface profile measurement of a new wiper blade; 50X objective lens

Surface profile measurement of a wiper blade after durability testing; 50X objective lens
Surface profile measurement of a wiper blade after durability testing; 50X objective lens

Olympus IMS

应用所使用的产品

具有出色精度和光学性能的LEXT™OLS5100激光扫描显微镜配备了让系统更加易于使用的智能工具。其能够快速高效完成亚微米级形貌和表面粗糙度的精确测量任务,既简化了工作流程又能让您获得可信赖的高质量数据。

Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.
Sorry, this page is not available in your country