Ripple Marks Formed in Die-Casting / 3D shape measurement using a laser microscope


Application

In the die casting process, molten metal flowing into the mold may harden before it is fused completely, producing shallow wrinkles on the die-cast surface. This phenomenon is known as ripple marks. The ripple marks are problematic because they distort the external appearance of the product and may cause damage or deformation when stress is applied.

The Olympus solution

Olympus' LEXT 3D laser scanning microscope makes it easy to accurately image a three-dimensional surface profile down to the micron level. Users can perform defect management using numerical surface roughness data, which is the best method for quality control. With the LEXT’s image stitching feature, users can create high-contrast images of the entire defect location. Moreover, because the microscope is contactless, the object’s surface will not be scratched.

Non-defective surface

laser_non-defective_surface_bf

laser_non-defective_surface_3D

Objective lens 20X, Zoom 1X; 6×3 stitching

Defective surface

laser_defective_surface_bf

laser_defective_surface_3D
 

Olympus IMS

应用所使用的产品

具有出色精度和光学性能的LEXT™OLS5100激光扫描显微镜配备了让系统更加易于使用的智能工具。其能够快速高效完成亚微米级形貌和表面粗糙度的精确测量任务,既简化了工作流程又能让您获得可信赖的高质量数据。